Abstract:
Biooxidation of refractory gold-bearing pyrite-arsenopyrite flotation concentrate was optimized and aburidance of predominant groups in the community ofthermophilic acidophilic chemolithotrophic microorganisms at various stages ofbioleaching was determined. The optimal parameters for growth and leaching/oxidation of the mineral components of the concentrate were pSH 1.4, 1.6-1.8; 47.5 degrees C; and the following salt concentrations in the liquid phase (g/L): K2HPO4.3H2O, 0.53; (NH4)2SO4, 1.6 and MgSO4.7H2O, 2.5 (or (NH4)2SO4, 1.23; ammophos, 0.41; KOH, 0.1) with 0.03% yeast extract. The optimal conditions resulted in high growth rate, high levels of iron andarsenic leaching, of Fe2+ and S(2-)/S0 oxidation, and predominance of Acidithiobacillus caldus, Sulfobacillus spp., and Ferroplasma spp. in the community.
Related Concept Videos
Microbial Leaching
Acid Mine Drainage
Bioreactor Controls-II
Bioreactor Controls-III
Methods of Medium Optimization
Batch vs Continuous Culture