Thermal properties and morphology changes in degradation process of poly(L-lactide-co-glycolide) matrices with

Artur Turek1,2, Janusz Kasperczyk1,2, Katarzyna Jelonek1

  • 1Centre of Polymer and Carbon Materials, Polish Academy of Sciences, Zabrze, Poland.

Related Concept Videos

Polymer Classification: Stereospecificity01:26

Polymer Classification: Stereospecificity

Polymerization generates chiral centers along the entire backbone of a polymer chain. Accordingly, the stereochemistry of the substituent group has a significant effect on polymer properties. Polymers formed from monosubstituted alkene monomers feature chiral carbons at every alternate position in the polymer backbone. Relative to the predominant orientation of substituents at the adjacent chiral carbons, the polymer can exist in three different configurations: isotactic, syndiotactic, and...
3.4K
Modified-Release Drug Delivery Systems: Rate-Programmed II01:19

Modified-Release Drug Delivery Systems: Rate-Programmed II

Rate-programmed drug delivery systems release drugs in a controlled manner to maintain therapeutic levels. Three main designs include reservoir, matrix, and hybrid systems.Reservoir systems consist of a drug core enclosed within a membrane that controls drug release. In non-swelling reservoir systems, polymers like ethyl cellulose or polymethacrylates are used. These do not hydrate in aqueous media and control release through membrane thickness, porosity, or insolubility. This type includes...
103
Types of Step-Growth Polymers: Polyesters01:20

Types of Step-Growth Polymers: Polyesters

The introduction of polyesters has brought major development to the textile industry. The wrinkle-free behavior of polyester blends has eliminated the need for starching and ironing clothes.
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
2.7K