Aim:
The aim of this study was to evaluate the flexural and μTBS of bulk-fill materials.
Study Design:
Bulk-fill materials SDR, X-trabase (XTR) and TetricEvoCeramBulkFill (EVO) were used in this study. To test flexural strength, 25x2x2mm samples were prepared and tested with three point bending test. To test the microtensile bond strength (μTBS), two blocks (4x4x4mm) were prepared for each material. In Group A+B, acid-etching was applied to the surface of one of these blocks and no acid-etching was applied in Group B. After applying bonding agent, two blocks were placed into the mold and composite resin (COMP; Tetric N-Ceram) was applied with incremental layering. To evaluate the μTBS of primary dentin, the bulk-fill materials were applied to flat dentin up to 4mm. The new blocks and the teeth were sectioned to obtain sticks and the sticks were loaded in tension until failure. Flexural and microtensile bond strength was calculated based on failure load.
Results:
The ranking of materials with regards to flexural strength values were SDR>XTR>EVO>COMP,respectively. In GroupA+B, the μTBS values were XTR>SDR>EVO and were XTR>EVO>SDR in GroupB (p>0.05). The μTBS values of these materials to dentin were XTR>EVO>SDR (p>0.05).
Conclusion:
Within the limitations of this study, the use of a bonding agent without acid-etching showed positive interactions between base materials and composite resin and there were no significant differences in μTBS of these materials to dentin.
More Related Videos
Related Concept Videos
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen...
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...