Electrical and rheological properties of sewage sludge--Impact of the solid content

C Ségalen1, E Dieudé-Fauvel1, J C Baudez1

  • 1Irstea, UR TSCF, Domaine des Palaquins, F-03150 Montoldre, France.

Water Research
|August 26, 2015
PubMed

Related Concept Videos

Slump Test01:20

Slump Test

The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
1.4K
Coagulation01:06

Coagulation

Colloidal solids are solid particles suspended in solution. They are usually negatively charged, attracting a compact primary layer of positively charged ions, which attract more counterions to form an electrical double layer. Electrostatic repulsion between the charged double layers prevents the particles from colliding, stabilizing the colloids. These solids are often undesirable because they can contain toxins that are difficult to remove. Coagulation is a technique that helps aggregate and...
1.7K
Superplasticizers01:30

Superplasticizers

Superplasticizers are advanced admixtures that enhance the workability of concrete by lowering the water content without compromising the strength of the material. These substances are highly effective water reducers, improving concrete flow, making it easier to work with, and enabling concrete to reach inaccessible areas or densely reinforced sections without mechanical vibration. The key components in superplasticizers are either sulfonated melamine or naphthalene formaldehyde condensates,...
420
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
1.3K
Factors Affecting Workability01:24

Factors Affecting Workability

The workability of concrete is a critical characteristic that influences the ease of mixing, handling, and finishing the concrete. It is affected by several factors including water content, aggregate properties, and admixtures like air entrainment. Water plays a fundamental role as it lubricates the concrete mix, facilitating easier movement and placement. However, the water requirement varies depending on the texture and shape of aggregates. Finer particles and angular, rough-textured...
358
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
551