Vapor-Phase Atomic Layer Deposition of Co9S8 and Its Application for Supercapacitors

Hao Li1, Yuanhong Gao1, Youdong Shao1

  • 1School of Advanced Materials, Shenzhen Graduate School, Peking University , Shenzhen 518055, China.

Nano Letters
|August 28, 2015
PubMed

Related Concept Videos

MOS Capacitor01:25

MOS Capacitor

A Metal-Oxide-Semiconductor (MOS) capacitor is a fundamental structure used extensively in semiconductor device technology, particularly in the fabrication of integrated circuits and MOSFETs (metal-oxide-semiconductor field-effect transistors). The MOS capacitor consists of three layers: a metal gate, a dielectric oxide, and a semiconductor substrate.
The metal gate is typically made from highly conductive materials such as aluminum or polysilicon. Beneath the metal gate lies a thin layer of...
1.8K
Capacitor With A Dielectric01:18

Capacitor With A Dielectric

Parallel plate capacitors consist of two conducting plates separated by a certain distance. However, it is mechanically difficult to hold the large plates parallel to each other without actual contact. Hence, a dielectric layer is commonly placed between the plates, which provides an easy solution for holding the plates together with a small gap and increases the capacitance of the capacitor.
Dielectrics are non-conducting materials with no free or loosely bound electrons. When a dielectric is...
5.4K
Dielectric Polarization in a Capacitor01:31

Dielectric Polarization in a Capacitor

The presence of a dielectric medium in a capacitor not only changes the voltage and capacitance but also affects the electric field. In general, dielectrics can be of two types: polar and nonpolar. In a polar dielectric, the positive and negative charges in the molecules are separated by a distance and hence have a permanent dipole moment. In contrast, no such charge separation exists in a nonpolar dielectric, however the nonpolar molecules get polarized in the presence of an external electric...
6.5K
Spherical and Cylindrical Capacitor01:26

Spherical and Cylindrical Capacitor

A spherical capacitor consists of two concentric conducting spherical shells of radii R1 (inner shell) and R2 (outer shell). The shells have  equal and opposite charges of +Q and −Q, respectively. For an isolated conducting spherical capacitor, the radius of the outer shell can be considered to be infinite.
Conventionally, considering the  symmetry, the electric field between the concentric shells of a spherical capacitor is directed radially outward. The magnitude of the field,...
7.1K
Energy Stored in a Capacitor01:12

Energy Stored in a Capacitor

When an archer pulls the string in a bow, he saves the work done in the form of elastic potential energy. When he releases the string, the potential energy is released as kinetic energy of the arrow. A capacitor works on the same principle in which the work done is saved as electric potential energy. The potential energy (UC) could be calculated by measuring the work done (W) to charge the capacitor.
5.1K
Capacitors and Capacitance01:18

Capacitors and Capacitance

A device consisting of two electrical conductors that are separated by a distance and used to store electrical charges is called a capacitor. The space between the conductors is either a vacuum or an insulating material, called a dielectric. Capacitors have many applications, ranging from filtering static from radio reception to energy storage in heart defibrillators.
When the conductors are two identical parallel plates, it is called a parallel plate capacitor. When battery terminals are...
10.2K