Improved compaction of dried tannery wastewater sludge

M Della Zassa1, M Zerlottin2, D Refosco2

  • 1Dept. of Industrial Engineering, University of Padua, Via Marzolo, 9, 35131 Padova, Italy.

Abstract

Related Concept Videos

Compacting Factor test01:22

Compacting Factor test

The compacting factor test is a method used to assess the workability of concrete. It is  especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
692
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
357
Slump Test01:20

Slump Test

The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
1.4K
Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
556
Drying Shrinkage01:21

Drying Shrinkage

When hardened concrete is exposed to air with a relative humidity of less than 100 percent, it begins to lose the free water within its capillaries. As this water evaporates, the water initially adsorbed onto the calcium silicate hydrates migrates towards these now empty spaces and eventually evaporates as well. Over time, as more water leaves, the volume of the concrete decreases, a phenomenon known as drying shrinkage.
A portion of this drying shrinkage can be reversed; if the concrete is...
466
Moisture Content and Bulking of Aggregate01:10

Moisture Content and Bulking of Aggregate

The moisture content of aggregates is a crucial factor in construction, particularly in concrete mixing, as it influences the total water required in the mix. Moisture content represents the water coated on the exterior surface of the aggregate existing in a saturated and surface-dry condition. The total water content of a moist aggregate is the sum of its moisture content and water absorption.
When aggregates are exposed to rain or sit in stockpiles, they absorb moisture, which must be...