Related Experiment Video
Updated: Apr 3, 2026

11:34
Subsurface Defect Localization by Structured Heating Using Laser Projected Photothermal Thermography
Published on: May 15, 2017
11.6K
Determination of defect densities from spatiotemporally resolved optical-laser induced damage measurements
Applied Optics
|September 15, 2015
Abstract:
A procedure is developed to retrieve defect densities of optical coatings and surfaces from spatiotemporally resolved optical-laser induced damage (STEREO-LID) measurements. In STEREO-LID, the temporal onset and location of nanosecond laser damage initiation is measured for each excitation event. The power of STEREO-LID relative to traditional damage tests resulting in damage probabilities is characterized with LID data from Monte Carlo simulations.