Related Experiment Video
Updated: Apr 3, 2026

Writing Bragg Gratings in Multicore Fibers
Published on: April 20, 2016
Reactive molten core fabrication of glass-clad Se(0.8)Te(0.2) semiconductor core optical fibers
Abstract:
Phosphate glass-clad optical fibers comprising amorphous Se(0.8)Te(0.2) semiconductor core were fabricated by a reactive molten core approach. The Se(0.8)Te(0.2) crystals were precipitated in core region by a postdrawing annealing process, which were confirmed by X-ray diffraction, micro-Raman spectra, electron probe X-ray micro-analyzer, and transmission electron microscope measurement results. A two-cm-long crystalline Se(0.8)Te(0.2) semiconductor core optical fiber, electrically contacted to external circuitry through the fiber end facets, exhibits a two-orders-of-magnitude change in conductivity between dark and illuminated states. The great discrepancy in light and dark conductivity suggests that such crystalline Se(0.8)Te(0.2) semiconductor core optical fibers have promising applications in optical switch and photoconductivity of optical fiber array.
Related Concept Videos
Fiber Reinforced Concrete
Semiconductors
Metals such as copper (Cu), zinc (Zn), or lead (Pb) have low resistivity and feature conduction bands that are either not fully occupied or overlap with the valence band, making a bandgap non-existent. This allows electrons in the highest energy levels of the valence band to easily transition to the conduction band upon gaining...
Metal-Semiconductor Junctions
Schottky Barriers
Schottky barriers arise when a metal with a work function (Φm) contacts a semiconductor with a different work function (Φs). Initially, electrons transfer until the Fermi levels of the metal and semiconductor align at equilibrium. For instance, if Φm > Φs, the semiconductor Fermi level is higher than the metal's before contact. The...