Electrodeposition and Screening of Photoelectrochemical Activity in Conjugated Polymers Using Scanning

Barak D B Aaronson1, Jesus Garoz-Ruiz2, Joshua C Byers1

  • 1Department of Chemistry, University of Warwick , Gibbet Hill Road, Coventry, CV4 7AL, United Kingdom.

Related Concept Videos

Photochemical Electrocyclic Reactions: Stereochemistry01:26

Photochemical Electrocyclic Reactions: Stereochemistry

The absorption of UV–visible light by conjugated systems causes the promotion of an electron from the ground state to the excited state. Consequently, photochemical electrocyclic reactions proceed via the excited-state HOMO rather than the ground-state HOMO. Since the ground- and excited-state HOMOs have different symmetries, the stereochemical outcome of electrocyclic reactions depends on the mode of activation; i.e., thermal or photochemical.
Selection Rules: Photochemical Activation
2.4K
Electrogravimetric Analysis: Overview01:30

Electrogravimetric Analysis: Overview

Electrogravimetric analysis measures the weight of an analyte deposited electrolytically onto a suitable working electrode. This method involves applying a potential to a pre-weighed electrode submerged in a solution, which results in the desired substance being deposited through reduction at the cathode or oxidation at the anode. The electrode's weight is recorded after deposition, and the difference in weight gives the analyte's weight in the solution.
To test the completeness of the...
923
Voltammetric Techniques: Linear-Scan (E vs Time)01:12

Voltammetric Techniques: Linear-Scan (E vs Time)

Polarography is a classical voltammetric technique used to analyze electrochemical reactions. This method applies a linear potential sweep to a dropping mercury electrode (DME), and the resulting current is measured. A dropping mercury electrode is commonly used as the working electrode in polarography. It consists of a capillary tube filled with mercury, where the tiny droplet forms at the tip. This droplet continuously drops from the capillary, creating a new electrode surface for each...
1.5K