Nanomechanical characterization of nanostructured bainitic steel: Peak Force Microscopy and Nanoindentation with AFM

Lucia Morales-Rivas1, Alejandro González-Orive2, Carlos Garcia-Mateo1

  • 1Department of Physical Metallurgy, National Center for Metallurgical Research (CENIM-CSIC), Avda. Gregorio del Amo 8, 28040 Madrid, Spain.

Scientific Reports
|November 26, 2015
PubMed