A critical review of the growth, drainage and collapse of foams

Jianlong Wang1, Anh V Nguyen1, Saeed Farrokhpay2

  • 1School of Chemical Engineering, University of Queensland, Brisbane, QLD 4072, Australia.

Related Concept Videos

Molecular Weight of Step-Growth Polymers01:08

Molecular Weight of Step-Growth Polymers

Step growth polymerization involves bi or multifunctional monomers. Bifunctional monomers react to form linear step growth polymers, whereas multifunctional monomers react to form non-linear or branched polymers.
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
3.0K
Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
568
Cavity Drainage and Flashings in Masonry walls01:20

Cavity Drainage and Flashings in Masonry walls

Typically, a cavity wall consists of two wythes separated by a gap of at least 2 inches, which may contain insulation while still maintaining a minimum clear space of 1 inch to facilitate adequate drainage. Advanced methods like the insertion of a continuous drainage mat can further reduce this space while ensuring effective moisture expulsion.
Weep holes, strategically placed at the base of the cavity, are critical for draining accumulated water. These openings are created by leaving head...
585
Efflorescence in Masonry01:25

Efflorescence in Masonry

Efflorescence in masonry walls appears as a fluffy crystalline powder, often white, resulting from water-soluble salts within the masonry or mortar. When water penetrates the masonry, it dissolves these salts and brings them to the surface, where they are deposited upon evaporation of water.
While initial efflorescence is common post-construction and can be cleaned with water and a brush, in certain instances, efflorescence can reappear and gradually diminish over time as salts are leached out...
432
Shrinkage in Concrete01:27

Shrinkage in Concrete

Shrinkage in concrete is primarily due to water loss from evaporation, hydration of cement, or carbonation, leading to a reduction in volume. The volumetric contraction results in volumetric strain in concrete. However, in practice, shrinkage is measured as linear strain, which is one-third of the volumetric strain.
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...