Related Experiment Video
Updated: Mar 27, 2026

Spark Plasma Sintering Apparatus Used for the Formation of Strontium Titanate Bicrystals
Published on: February 9, 2017
Effect of Defect Distribution on the Optical Storage Properties of Strontium Gallates with a Low-Dimensional Chain
Ting Wang1, Xuhui Xu1,2, Dacheng Zhou1,2
1School of Materials Science and Engineering, Kunming University of Science and Technology , Xuefu RD, Kunming 650093, P. R. China.
Abstract:
The low-dimensional structure of the SrGa2O4 host exhibits a self-activated long persistent luminescence related to the creation of the oxygen vacancies. Because of the unique structure of the SrGa2O4 with a chain of cations along the a crystal direction, the emission and trapping centers could be introduced easily when the metal ions of Bi(3+) are doped. Both the photoluminescence and long persistent luminescence are related to two efficient emission centers of Bi(3+) in the two different crystallographic Sr sites, while the photostimulated luminescence spectra exhibit only one emission center of Bi1 ions under excitation at 980 or 808 nm. The results indicate that the distribution of defects in the low-chain structure of the SrGa2O4 host plays a vital role in the capture and transfer processes of carriers, which has a profound influence on the luminescence performance of SrGa2O4:Bi(3+) as one of the electron-trapping materials.
More Related Videos
09:45Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
Published on: July 26, 2016
06:57Theoretical Calculation and Experimental Verification for Dislocation Reduction in Germanium Epitaxial Layers with Semicylindrical Voids on Silicon
Published on: July 17, 2020
Related Concept Videos
Imperfections in Crystal Structure: Stoichiometric Point Defects
Imperfections in Crystal Structure: Non-Stoichiometric Defects
Imperfections in Crystal Structure: Point, Line and Plane Defects
Three-Dimensional Analysis of Strain
Valence Bond Theory
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...