Related Experiment Video
Updated: Mar 26, 2026

In Vitro Evaluation of The Effects Of Er,Cr:YSGG and Diode Lasers Used on Titanium Cylinder
Published on: June 6, 2025
Longitudinal Effect of Surface Treatments Modified by NaOCl-Induced Deproteinization and Nd:YAG Laser on Dentin
Stella Renata Machado Silva Esteves1, Maria Filomena Rocha Lima Huhtala1, Ana Paula Martins Gomes1
11 Department of Restorative Dentistry, São José dos Campos School of Dentistry, University Estadual Paulista , SP, Brazil .
Objective:
The purpose of this study was to evaluate dentin permeability after dentin hypersensitivity treatments: fluoride, adhesive system, and collagen deproteinization with and without Nd:YAG laser exposure, and after erosive and abrasive challenges.
Materials And Methods:
Dentin permeability was assessed by measuring dentinal fluid flow using a permeability device. Eighty bovine dentin specimens (6 mm diameter/1 mm thickness) had permeability measured in the presence of the smear layer and after removal of the smear layer by ethylenediaminetetraacetic acid (EDTA). They were then divided into eight groups according to treatment (n = 10): Group C, control; Group L, Nd:YAG laser; Group F, fluoride; Group FL, fluoride plus Nd:YAG laser; Group A, adhesive; Group AL, adhesive plus Nd:YAG laser; Group D, 10% NaOCl plus adhesive; and group DL, NaOCl plus adhesive plus Nd:YAG laser. Nd:YAG laser was irradiated at 60 mJ/pulse/10 Hz/47.7 J/cm2/1 W and applied freehanded without contact for 60 sec. Permeability was measured 24 h after the treatments. The specimens were exposed to erosive and abrasive challenges for 5 days. Erosive challenge was done by immersion in Coca-Cola, four times a day/90 sec each. After the first and last erosive challenge of the day, the abrasive challenge was conducted by brushing the specimens (24,000 cycles/3.8 cm range/200 g weight), and permeability was measured again. Results were analyzed statistically using two factor ANOVA and Tukey tests (α = 0.05).
Results:
With the exception of groups FL and A, all treatments reduced permeability. A significant reduction in permeability was seen when the treatments were combined with laser exposure. The association of adhesive and Nd:YAG laser led to the lowest rate of permeability after 24 h. NaOCl-induced deproteinization associated with Nd:YAG laser showed the lowest permeability rate after erosive/abrasive challenges.
Conclusions:
Dentin hypersensitivity treatments reduced dentin permeability when associated with Nd:YAG laser, even after erosive/abrasive challenges.
More Related Videos
06:36Effects of Mechanical Methods Used in Peri-implantitis Treatment on Implant Surface Decontamination and Roughness
Published on: March 14, 2025
06:06Adjunctive Diode Laser Therapy and Probiotic Lactobacillus Therapy in the Treatment of Periodontitis and Peri-Implant Disease
Published on: May 9, 2022