Abstract:
In this study, cotton was bleached at low temperatures with an activated peroxide system which was established by incorporating a bleach activator, namely, N-[4-(triethylammoniomethyl)benzoyl]caprolactam chloride (TBCC) into an aqueous solution of hydrogen peroxide (H2O2). Experimental results showed that the bleaching performance was unexpectedly diminished as the TBCC concentration was increased over the range of 25-100g/L. Kinetic adsorption experiment indicated that this was most likely ascribed to the adsorptive interactions of TBCC and the in situ-generated compounds with cotton fibers. Such a limitation was especially fatal to cold pad-batch bleaching process of cotton in which a high TBCC concentration was often required. The results of this study may stimulate further research to avoid or overcome the limitation of the TBCC-activated peroxide system on low-temperature cotton bleaching.
More Related Videos
Related Concept Videos
Cycloaddition Reactions: MO Requirements for Photochemical Activation
Physical Methods for Controlling Microbial Growth: Temperature
Methods of Sterilization II: Chemical Methods
Using chemical sterilization rather than heat to clean out equipment is recommended. It eradicates and removes all bacteria,...
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...