Y-shaped ZnO Nanobelts Driven from Twinned Dislocations

Yuan Shi1, Shuhan Bao1, Run Shi1

  • 1Department of Materials Science and Engineering and Shenzhen Key Laboratory of Nanoimprint Technology, South University of Science and Technology, Shenzhen 518055, China.

Scientific Reports
|March 3, 2016
PubMed

Related Concept Videos

Ziegler–Natta Chain-Growth Polymerization: Overview01:17

Ziegler–Natta Chain-Growth Polymerization: Overview

Ziegler–Natta polymerization is another form of addition or chain‐growth polymerization used for synthesizing linear polymers over branched polymers. The catalyst used for polymerization is the Ziegler–Natta catalyst, named after Karl Ziegler and Giulio Natta, who developed it in 1953. This catalyst is an organometallic complex of titanium tetrachloride and triethyl aluminum, with the active form of the catalyst being an alkyl titanium compound. Using the Ziegler–Natta...
4.2K
Imperfections in Crystal Structure: Stoichiometric Point Defects01:26

Imperfections in Crystal Structure: Stoichiometric Point Defects

Schottky defects arise when some lattice points in a crystal, such as those in NaCl, remain unoccupied, creating lattice vacancies without disturbing the overall electrical neutrality of the crystal. This defect is common in ionic crystals where the positive and negative ions are similar in size, as seen in sodium chloride and cesium chloride. The presence of Schottky defects enables the crystal to conduct electricity to a small extent through an ionic mechanism. Electric fields cause nearby...
66
Imperfections in Crystal Structure: Point, Line and Plane Defects01:25

Imperfections in Crystal Structure: Point, Line and Plane Defects

A perfect crystal, in theory, has a uniform structure with the same unit cell and lattice points throughout. However, any deviation from this periodic arrangement is known as an imperfection or defect. These defects can be categorized into three types: point, line, and plane defects.Point defects occur when there is a deviation from the ideal due to missing atoms, displaced atoms, or additional atoms. These imperfections might occur due to imperfect packing during crystallization or because of...
54