Nanoporous silver cathode surface treated by atomic layer deposition of CeO(x) for low-temperature solid oxide fuel
Ke Chean Neoh1, Gwon Deok Han, Manjin Kim
1Renewable Energy System Laboratory, School of Mechanical Engineering, Korea University, 145 Anam-ro, Seongbuk-gu, Seoul 136-713, Korea.
Abstract:
We evaluated the performance of solid oxide fuel cells (SOFCs) with a 50 nm thin silver (Ag) cathode surface treated with cerium oxide (CeO(x)) by atomic layer deposition (ALD). The performances of bare and ALD-treated Ag cathodes were evaluated on gadolinia-doped ceria (GDC) electrolyte supporting cells with a platinum (Pt) anode over 300 °C-450 °C. Our work confirms that ALD CeO(x) treatment enhances cathodic performance and thermal stability of the Ag cathode. The performance difference between cells using a Ag cathode optimally treated with an ALD CeO(x) surface and a reference Pt cathode is about 50% at 450 °C in terms of fuel cell power output in our experiment. The bare Ag cathode completely agglomerated into islands during fuel cell operation at 450 °C, while the ALD CeO(x) treatment effectively protects the porosity of the cathode. We also discuss the long-term stability of ALD CeO(x)-treated Ag cathodes related to the microstructure of the layers.
More Related Videos
10:15Solar-Driven Electrochemical Green Fuel Production from CO2 and Water Using Ti3C2Tx MXene-Supported CuZn and NiCo Catalysts
Published on: November 7, 2025
07:13High Temperature Fabrication of Nanostructured Yttria-Stabilized-Zirconia YSZ Scaffolds by In Situ Carbon Templating Xerogels
Published on: April 16, 2017