Stabilizing a high-temperature electrochemical silver-carbonate CO2 capture membrane by atomic layer deposition of a
Peng Zhang1, Jingjing Tong1, Youngseok Jee1
1Department of Mechanical Engineering, University of South Carolina, Columbia, SC 29201, USA. huang46@cec.sc.edu.
Abstract:
A high-selectivity and high-flux electrochemical silver-carbonate dual-phase membrane was coated with a nanoscaled ZrO2 layer by atomic layer deposition (ALD) for stable CO2 capture at high-temperature (≥800 °C); the latter has an important implication for direct dry methane reforming with the captured CO2 and O2 for syngas production.
More Related Videos
12:47Preparation and Use of Photocatalytically Active Segmented Ag|ZnO and Coaxial TiO2-Ag Nanowires Made by Templated Electrodeposition
Published on: May 2, 2014
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited Zn1-xMgxO
Published on: July 31, 2016
Related Concept Videos
Electrodeposition
Electrodeposition can...
Colloidal precipitates