Related Experiment Video
Updated: Mar 17, 2026

Fabrication of Low Temperature Carbon Nanotube Vertical Interconnects Compatible with Semiconductor Technology
Published on: December 7, 2015
Temperature-dependent magnetic properties of Ni nanotubes synthesized by atomic layer deposition
Alejandro Pereira1, Juan L Palma1, Juliano C Denardin1
1Department of Physics, Universidad de Santiago de Chile and Center for the Development of Nanoscience and Nanotechnology, 9170124 Santiago, Chile.
Abstract:
Highly-ordered and conformal Ni nanotube arrays were prepared by combining atomic layer deposition (ALD) in a porous alumina matrix with a subsequent thermal reduction process. In order to obtain NiO tubes, one ALD NiCp2/O3 cycle was repeated 2000 times. After the ALD process, the sample is reduced from NiO to metallic Ni under hydrogen atmosphere. Their magnetic properties such as coercivity and squareness have been determined in a vibrating sample magnetometer in the temperature range from 5-300 K for applied magnetic fields parallel and perpendicular to the nanotube axis. Ni nanotubes synthesized by ALD provide a promising opportunity for potential applications in spintronics, data storage and bio-applications.