Related Experiment Video
Updated: Mar 17, 2026

Experimental Protocol to Investigate Particle Aerosolization of a Product Under Abrasion and Under Environmental Weathering
Published on: September 16, 2016
Potential Explosion Hazard of Carbonaceous Nanoparticles: Screening of Allotropes
Leonid A Turkevich1, Joseph Fernback1, Ashok G Dastidar2
1National Institute for Occupational Safety and Health, Division of Applied Research and Technology, 1090 Tusculum Avenue, MS-R7, Cincinnati, OH 45226 USA.
Abstract:
There is a concern that engineered carbon nanoparticles, when manufactured on an industrial scale, will pose an explosion hazard. Explosion testing has been performed on 20 codes of carbonaceous powders. These include several different codes of SWCNTs (single-walled carbon nanotubes), MWCNTs (multi-walled carbon nanotubes) and CNFs (carbon nanofibers), graphene, diamond, fullerene, as well as several different control carbon blacks and graphites. Explosion screening was performed in a 20 L explosion chamber (ASTM E1226 protocol), at a concentration of 500 g/m3, using a 5 kJ ignition source. Time traces of overpressure were recorded. Samples typically exhibited overpressures of 5-7 bar, and deflagration index KSt = V1/3 (dP/dt)max ~ 10 - 80 bar-m/s, which places these materials in European Dust Explosion Class St-1. There is minimal variation between these different materials. The explosive characteristics of these carbonaceous powders are uncorrelated with primary particle size (BET specific surface area).