Related Experiment Video
Updated: Mar 15, 2026

Force System with Vertical V-Bends: A 3D In Vitro Assessment of Elastic and Rigid Rectangular Archwires
Published on: July 24, 2018
Stiffness comparison of mushroom and straight SS and TMA lingual archwires
Luca Lombardo1, Antonella Carlucci1, Mario Palone2
1Postgraduate School of Orthodontics, University of Ferrara, Via Montebello 31, 44100, Ferrara, Italy.
Background:
The aim of this study is to investigate the relative stiffness of straight and mushroom lingual archwires of different diameters, cross sections and alloys, plotting their load/deflection graphs and using a modified three-point bending test.
Methods:
Fujita's mushroom archwires and straight lingual archwires of different diameters, cross sections and alloys were derived by a virtual set-up of an equal malocclusion and were cut at their straight distal portion. These distal portions were tested using a modified three-point bending test by an Instron 4467 dynamometer and the forces, were exerted at 1-mm deflection and were compared on each resulting load/deflection curve by means of ANOVA (p < 0.05).
Results:
All upper lingual mushroom wires exerted significantly lower forces than the straight wire. Lower mushroom archwires were stiffer than their upper counterparts, which were longer and featured inset bends. In the lower arch, similar levels of forces were recorded for the two types of wire. Load-deflection curves were higher for the straight wires, and stiffness increased proportionally with their diameter.
Conclusions:
The stiffness of an archwire is a function of its diameter, length and the alloy it is made from. In lower lingual wires, there is little difference in stiffness between mushroom and straight wires, but in upper wires, the straight version is considerably stiffer. The greater bearing effect exhibited by the straight wire in the working and finishing phases makes it less susceptible to bowing effect and therefore preferable for sliding mechanics during en masse retraction, particularly in the upper arch.
More Related Videos
Related Concept Videos
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55...
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Posttensioned Masonry Walls
Post-tensioned masonry walls use high-strength steel rods or flexible tendons to enhance the strength and efficiency of masonry structures. These elements are securely anchored to the foundation and extend vertically either within the cores of the masonry units or between the masonry wythes. The construction process involves building the wall with these tensioning elements in place and allowing the mortar to fully cure.
Following the curing process, the tensioning begins. Steel rods are...
Temperature Dependent Deformation
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Hooke's Law