Phase transformation strengthening of high-temperature superalloys

T M Smith1, B D Esser1, N Antolin2

  • 1Center for Electron Microscopy and Analysis, The Ohio State University, Columbus, Ohio 43212, USA.

Nature Communications
|November 23, 2016
PubMed