ZnO films formed by atomic layer deposition as an optical biosensor platform for the detection of Grapevine virus
Alla Tereshchenko1, Viktoriia Fedorenko2, Valentyn Smyntyna1
1Experimental Physics Department, Odesa National I. I. Mechnikov University, 42, Pastera, 65023, Odesa, Ukraine.
Abstract:
Novel sensitive optical biosensor for determination of Grapevine virus A-type (GVA) proteins (GVA-antigens) has been designed. This biosensor was based on thin films of Zinc Oxide (ZnO) deposited by atomic layer deposition (ALD). The ZnO-based films have demonstrated favorable surface-structural properties for the direct immobilization of antibodies against GVA-antigens in order to form a biosensitive layer sensitive to GVA-antigens. The immobilization was confirmed by intensity changes in the main near band emission (NBE) peak of ZnO and by the formation of intense photoluminescence band, discovered in the visible range around 425nm, caused by the immobilized proteins. The GVA-antigen detection was performed by the evaluation of changes and behavior of a corresponding luminescence band. The sensitivity of as-formed label-free biosensor towards the GVA-antigens was determined in the range from 1pg/ml to 10ng/ml; in addition, the selectivity of biosensor was evaluated.
More Related Videos
08:18Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application
Published on: October 3, 2015
08:22Ultrasensitive Detection of Biomarkers by Using a Molecular Imprinting Based Capacitive Biosensor
Published on: February 16, 2018