Related Experiment Video
Updated: Mar 8, 2026

Applying Dynamic Strain on Thin Oxide Films Immobilized on a Pseudoelastic Nickel-Titanium Alloy
Published on: July 28, 2020
Long-term time dependence of internal stress in lanthanum titanium oxide (H4) optical thin films
Abstract:
The time variation in the internal stress of optical thin films composed of lanthanum titanium oxide (H4) deposited by ion-beam assisted deposition (IAD) and electron beam deposition was observed over a period of 10 years after deposition, and it was found that the internal stresses in the optical thin films can be controlled by optimizing the IAD conditions. Both tensile stress and compressive stress could be created by IAD, and the chemical bonding state of Ti may affect the stress behavior. The network size of the chemical bonds may affect the stress direction.
Related Concept Videos
General State of Stress
Specifically, consider a tetrahedral element where one face, labeled XYZ, is perpendicular to the line OA, and the remaining faces align with the coordinate axes with point O as the origin. At any point, such as point O, the stress tensor can be used to determine the stress...
Plastic Behavior
Residual Stresses in Bending