New System of Shrinkage Measurement through Cement Mortars Drying

Carlos Morón1, Pablo Saiz2, Daniel Ferrández3

  • 1Sensors and Actuators Group, Department of Building Technology, Madrid Technical University, 28040 Madrid, Spain. carlos.moron@upm.es.

Related Concept Videos

Drying Shrinkage01:21

Drying Shrinkage

When hardened concrete is exposed to air with a relative humidity of less than 100 percent, it begins to lose the free water within its capillaries. As this water evaporates, the water initially adsorbed onto the calcium silicate hydrates migrates towards these now empty spaces and eventually evaporates as well. Over time, as more water leaves, the volume of the concrete decreases, a phenomenon known as drying shrinkage.
A portion of this drying shrinkage can be reversed; if the concrete is...
428
Shrinkage in Concrete01:27

Shrinkage in Concrete

Shrinkage in concrete is primarily due to water loss from evaporation, hydration of cement, or carbonation, leading to a reduction in volume. The volumetric contraction results in volumetric strain in concrete. However, in practice, shrinkage is measured as linear strain, which is one-third of the volumetric strain.
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
457
Mortar Properties01:17

Mortar Properties

Mortar properties encompass a range of characteristics crucial for construction and masonry work, including workability, water retention, bond strength, durability, compressive strength, volume change, and appearance. Workability refers to mortar's ability to be easily applied and manipulated without sagging or falling off surfaces, which is important for efficient masonry unit placement and alignment. Water retention is essential to prevent the mortar from losing moisture too quickly to...
540
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
698
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the...
854
Measurement of Air Content in Concrete01:23

Measurement of Air Content in Concrete

Air content measurement in concrete is critical for ensuring structural integrity and durability of concrete structures, especially in environments prone to severe weather conditions. Accurate air content analysis optimizes concrete's resistance to freeze-thaw cycles and enhances its workability and strength. Several methods are standardized under ASTM guidelines to measure the air content in fresh concrete, each suitable for different concrete types and conditions.
The pressure method,...