Robust Slippery Coating with Superior Corrosion Resistance and Anti-Icing Performance for AZ31B Mg Alloy Protection

Jialei Zhang1,2, Changdong Gu1,2, Jiangping Tu1,2

  • 1School of Materials Science and Engineering, State Key Laboratory of Silicon Materials, Zhejiang University , Hangzhou 310027, China.

Related Concept Videos

Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
29.0K
Accelerators01:17

Accelerators

Accelerators in concrete serve as admixtures to speed up the hardening process, enabling the concrete to achieve early strength faster. Although accelerators do not necessarily impact the time it takes concrete to set, they reduce this time in practice. A common accelerator is calcium chloride, which is particularly useful for hastening early strength development in cold weather or for rapid repair jobs that require quick heat generation after mixing.
The effectiveness of calcium chloride can...
322
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
635
Frost Resistant Concrete01:29

Frost Resistant Concrete

Concrete's susceptibility to frost damage during freeze-thaw cycles demands strategic measures to enhance its frost resistance. Employing techniques like air entrainment, adjusting the water-cement ratio, proper curing, and selecting appropriate aggregates are essential.
Introducing microscopic air bubbles into the concrete mix through air entrainment creates small voids that accommodate ice expansion, thereby reducing internal pressures and preventing cracking. The optimal amount of...
448