Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
504
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
374
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
360
Expansion and Contraction in Masonry Walls01:19

Expansion and Contraction in Masonry Walls

Masonry walls are subject to slight expansion and contraction due to variations in temperature and moisture. Thermal movement in masonry is relatively straightforward to measure and plan for. On the other hand, moisture movement poses more of a challenge. New clay masonry units typically absorb water and expand over time under normal environmental conditions. Conversely, new concrete masonry units tend to shrink as they lose the excess moisture acquired during their production process.
To...
1.4K
Masonry Cavity Walls01:26

Masonry Cavity Walls

Cavity walls feature a hollow space between the outer and inner wythes, connected only by corrosion-resistant metal ties. When water seeps through the outer wythe, it descends within this cavity, intercepted by flashing and eventually exiting through weep holes. To enhance moisture resistance, the inner wythe's cavity side often receives damp-proofing, doubling as an air barrier. The cavity can also house insulation to mitigate heat transfer.
Maintaining a clean cavity during construction...
1.5K
Cavity Drainage and Flashings in Masonry walls01:20

Cavity Drainage and Flashings in Masonry walls

Typically, a cavity wall consists of two wythes separated by a gap of at least 2 inches, which may contain insulation while still maintaining a minimum clear space of 1 inch to facilitate adequate drainage. Advanced methods like the insertion of a continuous drainage mat can further reduce this space while ensuring effective moisture expulsion.
Weep holes, strategically placed at the base of the cavity, are critical for draining accumulated water. These openings are created by leaving head...
518