Environmental Temperature Drastically Affects Flexural Fatigue Resistance of Nickel-titanium Rotary Files
Nicola Maria Grande1, Gianluca Plotino2, Enrico Silla1
1Catholic University of Sacred Heart, Rome, Italy.
Introduction:
The aim of the present study was to analyze how a low environmental temperature can affect the fatigue life of instruments made by different types of heat-treated nickel-titanium alloys.
Methods:
The flexural cyclic fatigue of 40 new specimens for each of the following systems was tested for cyclic fatigue resistance: ProTaper Universal F2 (Dentsply Maillefer, Ballaigues, Switzerland), ProTaper Gold F2 (Dentsply Tulsa Dental Specialties, Tulsa, OK), Twisted Files SM2 (SybronEndo, Orange, CA), Mtwo #25.06 (VDW, Munich, Germany), and Vortex Blue #30.04 and #40.06 (Dentsply Tulsa Dental Specialties). Instruments were tested at 2 different environmental temperatures: 20°C (±2°C) for room temperature (RT) group and -20°C (±2°C) for the cooled environment (CE) group (n = 20). The number of cycles to failure (NCF) and the length of the fractured fragment (FL) were recorded. The means and standard deviations of NCF and FL were then calculated; NCF data were statistically analyzed using a paired t test between groups RT and CE for each instrument tested (P < .05), whereas FL data were analyzed using analysis of variance (P < .05).
Results:
The mean NCF values measured were significantly higher for the CE groups than the RT groups in all the systems tested (P < .05). The increase in cyclic fatigue resistance varied from 274%-854%. No differences in FL were registered among the different groups (P < .05).
Conclusions:
A low environmental temperature determines a drastic increase in the flexural fatigue resistance of NiTi endodontic instruments manufactured with traditional alloy and different heat treatments.
More Related Videos
Related Concept Videos
Fatigue
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55...
Temperature Dependent Deformation
Stress Concentrations in Circular Shafts
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Thermal Stress