Slump Test01:20

Slump Test

The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
1.0K
Design Example: Maintaining Level of an Embankment01:19

Design Example: Maintaining Level of an Embankment

Constructing a roadway embankment over uneven terrain requires precise leveling to ensure stability and proper drainage. Surveyors use a leveling instrument and staff to calculate ground elevations and determine the required fill material at each point along the embankment alignment.The process begins by positioning a leveling instrument near a benchmark with a known elevation. A backsight reading establishes the instrument height, which serves as a reference for subsequent measurements. A...
482
Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
670
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
418
Non-destructive Tests for Concrete Strength01:12

Non-destructive Tests for Concrete Strength

The rebound hammer test, also known as the Schmidt hammer test, is a non-destructive technique for evaluating the hardness of concrete and, indirectly, the strength of concrete. It operates on the principle that the rebound of a spring-driven mass from a concrete surface correlates to the surface's hardness. The device comprises a mass within a tubular housing, a spring mechanism, and a plunger that strikes the concrete. Upon release, the energy imparted to the mass by the spring causes it...
688
Compacting Factor test01:22

Compacting Factor test

The compacting factor test is a method used to assess the workability of concrete. It is  especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
650