Effect of air-blowing duration on the bond strength of current one-step adhesives to dentin
Jiale Fu1, Pipop Saikaew2, Shimpei Kawano3
1General Dentistry, Department of Endodontics, School and Hospital of Stomatology, China Medical University, No. 117 Nanjing Street, Heping District, 110002 Shenyang, Liaoning Province, China.
Objectives:
To evaluate the influence of different air-blowing durations on the micro-tensile bond strength (μTBS) of five current one-step adhesive systems to dentin.
Methods:
One hundred and five caries-free human molars and five current one-step adhesive systems were used: ABU (All Bond Universal, Bisco, Inc.), CUB (CLEARFIL™ Universal Bond, Kuraray), GPB (G-Premio BOND, GC), OBA (OptiBond All-in-one, Kerr) and SBU (Scotchbond Universal, 3M ESPE). The adhesives were applied to 600 SiC paper-flat dentin surfaces according to each manufacturer's instructions and were air-dried with standard, oil-free air pressure of 0.25MPa for either 0s, 5s, 15s or 30s before light-curing. Bond strength to dentin was determined by using μTBS test after 24h of water storage. The fracture pattern on the dentin surface was analyzed by SEM. The resin-dentin interface of untested specimens was visualized by panoramic SEM image. Data from μTBS were analyzed using two-way ANOVA (adhesive vs. air-blowing time), and Games-Howell (a=0.05).
Results:
Two-way ANOVA revealed a significant effect of materials (p=0.000) and air-blowing time (p=0.000) on bond strength to dentin. The interaction between factors was also significantly different (p=0.000). Maximum bond strength for each system were recorded, OBA/15s (76.34±19.15MPa), SBU/15s (75.18±12.83MPa), CUB/15s (68.23±16.36MPa), GPB/30s (55.82±12.99MPa) and ABU/15s (44.75±8.95MPa). The maximum bond strength of OBA and SUB were significantly higher than that of GPB and ABU (p<0.05).
Significance:
The bond strength of the current one-step adhesive systems is material-dependent (p=0.000), and was influenced by air-blowing duration (p=0.000). For the current one-step adhesive systems, higher bond strengths could be achieved with prolonged air-blowing duration between 15-30s.
More Related Videos
05:30Roughness Impact of Piezoelectric Dental Scaler on Two Distinct Flowable Composite Filling Materials
Published on: January 10, 2025
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Related Concept Videos
Effects of Air-entrainment in Concrete
Bonding and Strength of Aggregate
Chemical Bonds
Atoms participate in a chemical bond formation to acquire a completed valence-shell electron configuration similar to that of the noble gas nearest to it in atomic number. Ionic, covalent, and metallic bonds are some of the important types of chemical bonds. Bond energy and bond length determine the strength of a chemical bond.
Types of Chemical Bonds
An ionic bond is formed due to electrostatic attraction between cations and anions. Often, the ions are formed by the transfer of electrons...
Air-entraining Agents
Bond Energies and Bond Lengths