Morphological explanation of high tear resistance of EPDM/NR rubber blends
Christoph Gögelein1, Henri Jacob Hubert Beelen, Martin van Duin
1Polymer Testing, ARLANXEO Deutschland GmbH, Kaiser-Wilhelm-Allee 40, 51369 Leverkusen, Germany. christoph.goegelein@arlanxeo.com.
Abstract:
The fatigue properties of cross-linked blends of ethylene propylene diene rubber (EPDM) with low natural rubber (NR) content and reinforced with carbon black (CB) are studied. It is found that such EPDM/NR compounds have superior crack growth resistance and fatigue lifetime. For low NR contents, transmission electron microscopy reveals that the NR phase forms small droplets of 20-50 nm. Remarkably, these droplets are even smaller than the primary CB particles. Atomic force microscopy shows that the the NR phase droplets have a higher loss factor and a smaller elastic modulus than the surrounding EPDM matrix. Rheometer measurements are used to study the effect of the phase morphology on the rubber mechanical properties. These rheological data are compared with the prediction of the Eshelby model describing the effect of elastic inclusions on solids. A complex interplay between the rubber phase morphology and the solubility of both the sulfur cross-linking system and CB is observed, which cannot be predicted theoretically. It is proposed that the soft NR droplets effectively inhibit the crack propagation in the EPDM matrix.
Related Concept Videos
Polymer Classification: Architecture
Logarithmic Differentiation
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Olefin Metathesis Polymerization: Overview
Ruthenium-based Grubbs catalyst is the most commonly used catalyst for olefin metathesis polymerization. Grubbs catalyst consists of a...
Free-Radical Chain Reaction and Polymerization of Alkenes
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...