In-plane anisotropy and twin boundary effects in vanadium nitride under nanoindentation

Tao Fu1, Xianghe Peng2,3, Cheng Huang1

  • 1College of Aerospace Engineering, Chongqing University, Chongqing, 400044, China.

Scientific Reports
|July 8, 2017