Strain-induced phase transformation behavior of stabilized zirconia ceramics studied via nanoindentation
Erqiang Liu1, Gesheng Xiao2, Wufei Jia2
1College of Applied Science, Taiyuan University of Science and Technology, Taiyuan 030024, China.
Abstract:
To study the tetragonal-to-monoclinic (T-M) phase transformation behavior under different strain rates and indentation depths, nanoindentation tests were performed on stabilized zirconia ceramics with Continuous Stiffness Measurements. The results indicate decreased phase transformation velocities at both lower and higher strain rates, but increased velocity under medium strain rate during loading. The phase transformation process is sensitive to Ṗ/P but the final volume fractions are almost identical (45%). Furthermore, most of the phase transformation is completed during a short initial time followed by slight linear increase of the M-phase volume fraction with holding time. The phase transformation continuously slowed with increasing indentation depth when indented with a constant strain rate.
More Related Videos
08:29Multi-material Ceramic-Based Components – Additive Manufacturing of Black-and-white Zirconia Components by Thermoplastic 3D-Printing (CerAM - T3DP)
Published on: January 7, 2019
07:13High Temperature Fabrication of Nanostructured Yttria-Stabilized-Zirconia YSZ Scaffolds by In Situ Carbon Templating Xerogels
Published on: April 16, 2017