Promoted photoelectrocatalytic hydrogen evolution of a type II structure via an Al2O3 recombination barrier layer
Yajun Wang1, Weikun Bai, Haiquan Wang
1State Key Laboratory of Heavy Oil Processing, China University of Petroleum, Beijing 102249, China. jianggy@cup.edu.cn.
Abstract:
Constructing a semiconductor type II structure is an effective way to enhance the photogenerated charge separation efficiency. The separation and migration of interfacial photogenerated carriers is a key factor, which influences the photocatalytic activity. In this study, a conformal Al2O3 recombination barrier layer was introduced at the interface between TiO2 nanowires and CdSe nanoparticles, and the application of this composite in photoelectrocatalytic (PEC) hydrogen production was explored. Under visible-light irradiation, the photocurrent response and PEC hydrogen evolution performance increased step-by-step from TiO2 to the Al2O3/TiO2 and CdSe/Al2O3/TiO2 nanowire arrays. Moreover, the H2 evolution rate of CdSe/Al2O3/TiO2 was much higher than that of a different configuration, Al2O3/CdSe/TiO2. The enhanced PEC hydrogen evolution performance was attributed to the prevention of the interfacial charge recombination caused by the Al2O3 recombination barrier layer. Our results may shed new light on developing novel and highly efficient photocatalysts using rational interface design.
Related Concept Videos
Reduction of Alkenes: Catalytic Hydrogenation
Metals like palladium, platinum, and nickel are commonly used in their solid forms — fine powder on an inert surface. As these catalysts remain insoluble in the reaction mixture, they are referred to as heterogeneous catalysts.
The hydrogenation process takes place on the...
Reduction of Alkenes: Asymmetric Catalytic Hydrogenation
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...
Catalysis