Correlation Factor Study of Small Punch Creep Test and Its Life Prediction

Cheng Wen1, Tong Xu2, Kaishu Guan3

  • 1School of Mechanical and Power Engineering, East China University of Science and Technology, No. 130 Meilong Street, Xuhui District, Shanghai 200030, China. wen904437954@163.com.

Related Concept Videos

Factors Affecting Creep01:28

Factors Affecting Creep

In normal-weight aggregate concrete, the hardened cement paste is the primary contributor to creep, whereas the aggregates, being stiffer than the cement paste, are more resilient to stress-induced deformation. The stiffness of the aggregates is defined by their modulus of elasticity, and the more voluminous they are in the concrete, the less it will creep.
Further, the water/cement ratio is critical, as a lower ratio increases concrete strength, thus reducing creep. The strength of the...
481
Fatigue Strength of Concrete01:22

Fatigue Strength of Concrete

Fatigue, in the context of materials science and engineering, refers to the weakening or failure of a material caused by repeatedly applied loads, even if these loads are below the strength limit of the material. Fatigue strength in concrete is a critical property that influences its durability and longevity. Concrete can fail in two ways due to fatigue. Static fatigue or creep rupture occurs under a constant load or one that increases slowly. The other failure mode is due to cyclical or...
623
Creep in Concrete01:22

Creep in Concrete

Creep refers to the time-dependent increase in strain under a sustained load, excluding other time-dependent deformations associated with shrinkage, swelling, and thermal expansion in concrete. The primary mechanism behind creep involves the loss of physically adsorbed water from the calcium silicate hydrate within the hydrated cement paste. This process is further exacerbated by concrete's non-linear stress-strain relationship, microcrack development in the interfacial transition zone, and...
1.4K
Impact Strength of Concrete01:21

Impact Strength of Concrete

Impact strength in concrete is a critical measure that reflects the material's capability to endure the forces applied during pile driving and when supporting machinery foundations that experience impulsive loads. It is also essential when handling precast concrete components to prevent accidental damage. The impact strength is assessed by observing the concrete's resistance to repeated impacts and energy absorption capacity. A key indicator of significant damage to concrete is when it...
651
Effects of Creep01:25

Effects of Creep

Creep in concrete, the gradual deformation under prolonged stress, significantly impacts the integrity of structures. For reinforced concrete beams, it can be a vital design consideration, as it increases deflection, sometimes necessitating additional design measures. In columns, especially slender ones under eccentric loads, creep can cause buckling, compromising their stability. However, creep can be beneficial in indeterminate structures by mitigating stresses that arise from shrinkage,...
475
Behavior of Concrete Under Compressive Load01:23

Behavior of Concrete Under Compressive Load

Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
689