Characterisation of lattice damage formation in tantalum irradiated at variable temperatures
I Ipatova1,2, P T Wady2, S M Shubeita2
1School of Materials, The University of Manchester, Manchester, U.K.
Abstract:
The formation of radiation-induced dislocation loops and voids in tantalum at 180(2), 345(3) and 590(5)°C was assessed by 3MeV proton irradiation experiments and subsequent damage characterisation using transmission electron microscopy. Voids formed at 345(3)°C and were arranged into a body centred cubic lattice at a damage level of 0.55 dpa. The low vacancy mobility at 180(2)°C impedes enough vacancy clustering and therefore the formation of voids visible by TEM. At 590(5)°C the Burgers vector of the interstitial-type dislocation loops is a<100>, instead of the a/2 <111> Burgers vector characteristic of the loops at 180(2) and 345(3)°C. The lower mobility of a<100> loops hinders the formation of voids at 590(5)°C up to a damage level of 0.55 dpa.
More Related Videos
09:18Laser-heating and Radiance Spectrometry for the Study of Nuclear Materials in Conditions Simulating a Nuclear Power Plant Accident
Published on: December 14, 2017
08:31Sample Preparation and Experimental Design for In Situ Multi-Beam Transmission Electron Microscopy Irradiation Experiments
Published on: June 27, 2022