Investigation of Interaction between Dislocation Loop and Coherent Twin Boundary in BCC Ta Film during
Cheng Huang1, Xianghe Peng2,3, Bo Yang4
1College of Aerospace Engineering, Chongqing University, Chongqing 400044, China. huangcheng@cqu.edu.cn.
Abstract:
In this work, the interaction between dislocation loop (DL) and coherent twin boundary (CTB) in a body-centered cubic (BCC) tantalum (Ta) film during nanoindentation was investigated with molecular dynamics (MD) simulation. The formation and propagation of <111> full DLs in the nanotwinned (nt) Ta film during the indentation was observed, and it was found that CTB can strongly affect the stress distribution in the Ta film, and thus change the motion and type of dislocations. There are three kinds of mechanisms for the interaction between DL and CTB in a twinned BCC Ta film: (i) dislocation absorption, (ii) dislocation desorption, and (iii) direct slip transmission. The nucleation of twin boundary dislocations and the formation of the steps in CTB were also observed during the indentation. The mechanisms presented in this work can provide atomic images for understanding the plastic deformation of BCC metals with mirror-symmetry grain boundary structures, and provide available information for the evaluation and design of high-performance nt BCC metallic thin film coatings.
More Related Videos
Related Concept Videos
Atomic Force Microscopy
The AFM Probe
The probe is regarded as the heart of any AFM setup and comprises the...
Lattice Centering and Coordination Number
Types of Unit Cells
Imagine taking a large number of identical...