Related Experiment Video
Updated: Feb 19, 2026

09:45
Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
Published on: July 26, 2016
12.8K
Publisher Correction: Atomic-scale engineering of ferroelectric-ferromagnetic interfaces of epitaxial perovskite
Simon Hausmann1, Jingfan Ye1, Toshihiro Aoki2
1Technische Universität München, Physik-Department, Lehrstuhl für Neutronenstreuung, James-Franck-Strasse 1, D-85748, Garching, Germany.
Scientific Reports
|November 12, 2017
Abstract:
A correction to this article has been published and is linked from the HTML version of this paper. The error has been fixed in the paper.
Related Concept Videos
Magnetostatic Boundary Conditions
1.7K
An electric field suffers a discontinuity at a surface charge. Similarly, a magnetic field is discontinuous at a surface current. The perpendicular component of a magnetic field is continuous across the interface of two magnetic mediums. In contrast, its parallel component, perpendicular to the current, is discontinuous by the amount equal to the product of the vacuum permeability and the surface current. Like the scalar potential in electrostatics, the vector potential is also continuous...
1.7K
Ferromagnetism
3.2K
Materials like iron, nickel, and cobalt consist of magnetic domains, within which the magnetic dipoles are arranged parallel to each other. The magnetic dipoles are rigidly aligned in the same direction within a domain by quantum mechanical coupling among the atoms. This coupling is so strong that even thermal agitation at room temperature cannot break it. The result is that each domain has a net dipole moment. However, some materials have weaker coupling, and are ferromagnetic at lower...
3.2K