Effect of water storage on flexural strength of silorane and methacrylate-based composite resins
Narges Panahandeh1, Hassan Torabzadeh1, Hani Naderi2
1Dental Research Center, Research Institute of Dental Sciences, Shahid Beheshti University of Medical Sciences, Tehran, Iran.
Objectives:
This study assessed the effect of water storage on the flexural strength (FS) of low shrinkage composites.
Materials And Methods:
A total of 165 bar-shaped specimens (2 × 2 × 25 mm) were fabricated of 2 low shrinkage composites (Filtek P90 [3M ESPE], GC Kalore [GC International]) and a conventional methacrylate-based composite (Filtek Z250 [3M ESPE]). The specimens were subjected to 3-point bending test at 6 time intervals, namely: immediately after curing, at 24 hours, 1 week, 1 month, 6 months, and 1 year following storage in wet and dry conditions. The FS of the specimens were measured by applying compressive load at a crosshead speed of 1.0 mm/min. Data was analyzed using 3-way analysis of variance (ANOVA) and Tukey's test.
Results:
Three-way ANOVA revealed significant interactions between time, type of composite, and storage condition (p = 0.001). Tukey's multiple comparison test revealed significant reductions in FS of all composites after 6 months and 1 year of storage in distilled water compared to dry condition.
Conclusions:
Filtek P90 showed the highest and GC Kalore showed the lowest FS after 1 year storage in distilled water. The immediate high strength of Filtek Z250 significantly decreased at 1 year and its final value was lower than that of Filtek P90.
More Related Videos
07:15A Testing Platform for Durability Studies of Polymers and Fiber-reinforced Polymer Composites under Concurrent Hygrothermo-mechanical Stimuli
Published on: December 11, 2014
05:30Roughness Impact of Piezoelectric Dental Scaler on Two Distinct Flowable Composite Filling Materials
Published on: January 10, 2025
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
Effect of Sea Water on Concrete
Concrete in areas between tide marks,...
Accelerated Curing of Concrete
Relation Between Tensile Strength and Compressive Strength of Concrete