Fractographic Analysis of a Split Tooth Presenting Radiographically as a Horizontal Root Fracture in an Unrestored

Unni Krishnan1, Alex Moule1, Shaji Michael2

  • 1School of Dentistry, The University of Queensland, Brisbane, Queensland, Australia.

Journal of Endodontics
|December 26, 2017
PubMed
Abstract

Related Concept Videos

Molar Mass01:54

Molar Mass

The identity of a substance is defined not only by the types of atoms or ions it contains but by the quantity of each type of atom or ion. For example, water, H2O, and hydrogen peroxide, H2O2, are alike in that their respective molecules are composed of hydrogen and oxygen atoms. However, because a hydrogen peroxide molecule contains two oxygen atoms, as opposed to the water molecule, which has only one, the two substances exhibit very different properties.
87.2K
Tooth Anatomy01:21

Tooth Anatomy

The human tooth enables us to eat a variety of foods, speak clearly, and even aid in shaping our faces. Teeth are composed of various elements that work together. Here's a detailed look at the anatomy of a human tooth.
The Crown, Neck, and Root
The visible part of the tooth is referred to as the crown. It's covered by enamel, the hardest substance in the human body. The crown is uniquely shaped for each type of tooth, allowing for different functions such as cutting, tearing, or...
2.3K
Applications of the Ideal Gas Law: Molar Mass, Density, and Volume03:43

Applications of the Ideal Gas Law: Molar Mass, Density, and Volume

The volume occupied by one mole of a substance is its molar volume. The ideal gas law, PV = nRT,  suggests that the volume of a given quantity of gas and the number of moles in a given volume of gas vary with changes in pressure and temperature. At standard temperature and pressure, or STP (273.15 K and 1 atm), one mole of an ideal gas (regardless of its identity) has a volume of about 22.4 L — this is referred to as the standard molar volume.
63.7K
Horizontal Gene Transfer01:27

Horizontal Gene Transfer

Horizontal gene transfer (HGT) is a process where genetic material moves between organisms within the same generation, unlike vertical gene transfer, which occurs from parent to offspring. HGT plays a crucial role in microbial evolution, adaptation, and survival, particularly in shared environments like the human gut.Mobile genetic elements such as plasmids, prophages, integrons, insertion sequences, and transposons facilitate this process. HGT occurs through three primary mechanisms:...
2.4K
Introduction to Horizontal Curves01:19

Introduction to Horizontal Curves

Horizontal curves are essential in highway and railroad design, ensuring smooth and safe transitions between straight path segments, or tangents. These curves allow vehicles to maintain speed without abrupt changes, minimizing accidents and improving travel efficiency.A horizontal curve is typically defined by its geometric relationship to two tangents that meet at an intersection point (P.I.), where a simple curve is introduced to connect them. The back tangent refers to the initial tangent...
765
Horizontal Curve: Problem Solving01:03

Horizontal Curve: Problem Solving

A horizontal curve is characterized by its radius, intersection angle, and stationing of key points. In this case, the radius is 400 meters, and the angle of intersection is 30 degrees, with the station of the point of curvature (P.C.) at 0 + 150 meters. The goal is to determine the station values at the point of intersection (P.I.), point of tangency (P.T.), and midpoint of the curve, as well as the length of the long chord.The process begins with calculating the tangent distance (T) and the...
426