Related Experiment Video
Updated: Feb 16, 2026

Impact of Fabrication Techniques and Polishing Procedures on Surface Roughness of Denture Base Resins
Published on: January 17, 2025
Efficacy of Denture Cleansers on Impact Strength of Heat polymerized Acrylic Resins
Mallikarjuna Ragher1, Uma Mayoor Prabhu2, Jaya Prakash Ittigi3
1Department of Prosthodontics, Yenepoya Dental College, Yenepoya University, Mangalore, Karnataka, India.
Purpose:
The study was aimed to compare and evaluate the changes in the impact strength of heat cure denture base resins when treated using denture cleansers.
Methodology:
Study was conducted with sample size of 40 and dimesion 65 mm length, 10 mm width, and 3 mm thickness as per the ISO 1567. Distilled water has been used as control group, in which 10 samples were immersed of 40 samples. Of remaining 30 samples, 10 were treated with Clinsodent, 10 were treated with VI-Clean, and 10 were treated with Clanden denture cleansers. The impact strength of these specimens from each group was tested with the help of Charpy-type pendulum impact strength tester. The energy absorbed to fracture the specimens was recorded, and impact strength was calculated and was analyzed using Kruskal-Wallis ANOVA and Mann-Whitney test.
Results:
Impact strength of samples was significantly reduced after immersion in denture cleansers Clinsodent, VI-Clean, and Clanden solutions when compared to control group.
Conclusion:
Clinsodent, VI-Clean, and Clanden denture cleansers decrease the impact strength of heat cure denture base resin after immersion. Hence, the study concludes that denture cleansers should be used with caution and advised to follow manufacturer's instructions.
Related Concept Videos
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Impact Strength of Concrete
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Self-Efficacy
Specific Heat
For example, increasing the temperature of one gram of water by 1°C requires one calorie of heat energy and can be written as 1 cal/g-°C, or...
Quantifying Heat