A Reference-Free and Non-Contact Method for Detecting and Imaging Damage in Adhesive-Bonded Structures Using
Timotius Yonathan Sunarsa1, Pouria Aryan2, Ikgeun Jeon3
1Department of Civil and Environmental Engineering, KAIST, 291 Dahakro, Yuseong-gu, Daejeon 34141, Korea. timotisun@kaist.ac.kr.
Abstract:
Adhesive bonded structures have been widely used in aerospace, automobile, and marine industries. Due to the complex nature of the failure mechanisms of bonded structures, cost-effective and reliable damage detection is crucial for these industries. Most of the common damage detection methods are not adequately sensitive to the presence of weakened bonding. This paper presents an experimental and analytical method for the in-situ detection of damage in adhesive-bonded structures. The method is fully non-contact, using air-coupled ultrasonic transducers (ACT) for ultrasonic wave generation and sensing. The uniqueness of the proposed method relies on accurate detection and localization of weakened bonding in complex adhesive bonded structures. The specimens tested in this study are parts of real-world structures with critical and complex damage types, provided by Hyundai Heavy Industries® and IKTS Fraunhofer®. Various transmitter and receiver configurations, including through transmission, pitch-catch scanning, and probe holder angles, were attempted, and the obtained results were analyzed. The method examines the time-of-flight of the ultrasonic waves over a target inspection area, and the spatial variation of the time-of-flight information was examined to visualize and locate damage. The proposed method works without relying on reference data obtained from the pristine condition of the target specimen. Aluminum bonded plates and triplex adhesive layers with debonding and weakened bonding were used to examine the effectiveness of the method.
Related Concept Videos
Covalent Bonding and Lewis Structures
Spin–Spin Coupling: One-Bond Coupling
Spin–Spin Coupling: Two-Bond Coupling (Geminal Coupling)
The central atom need not be NMR-active because its electrons are affected by the electron polarization of the spin-active atoms. However, spin information is transmitted less effectively than in one-bond coupling, and 2J values are usually weaker than 1J values. The energy of...
Spin–Spin Coupling: Three-Bond Coupling (Vicinal Coupling)
The extent of coupling depends on the C‑C bond length, the two H‑C‑C angles, any electron-withdrawing substituents, and the dihedral angle between the involved orbitals. The...
Transducer Mechanism: G Protein–Coupled Receptors
GPCRs are also called heptahelical,...
Structure and Bonding of Alkenes
Doubly bonded carbons are sp2 hybridized and have a trigonal planar geometry. The double bond is composed of a σ bond formed by the overlap of hybrid orbitals and a π bond produced by the lateral overlap of unhybridized 2p orbitals on both the carbons. Each carbon atom is...