Effect of Coloring of Zirconia Framework and Ceramic Veneer on Adhesion of Interfacial Surfaces Determined Using
Purpose:
The aim of this study was to investigate the effect of coloring on the interfacial surface adhesion between a zirconia framework and ceramic veneer using three-point flexural bonding strength.
Materials And Methods:
A total of 40 zirconia bars (Zirlux ST1; DE Healthcare) were cut and divided into two groups of 20 (Groups 1 and 2). The two groups were then further split and divided into four groups of 10 each (Groups 1a, 1b, 2a, and 2b). Groups 1a and 1b tested adhesion of uncolored zirconia and two different shades of ceramic veneer, and Groups 2a and 2b tested adhesion of zirconia colored with two different coloring liquids and one shade of ceramic veneer.
Results:
Some coloring liquids used to color zirconia can significantly affect the bond strength between zirconia and the veneer, whereas ceramic veneer shades do not influence adhesion.
Conclusion:
Bonding strength between zirconia framework and ceramic veneer is affected by the coloring of the zirconia.
Related Concept Videos
Bonding and Strength of Aggregate
Veneer
Other veneering techniques include plain-slicing, quarter-slicing, and rift-slicing. These...
Bond Energies and Bond Lengths
Ionic Bonds
When atoms gain or lose electrons to achieve a more stable electron configuration they form ions. Ionic bonds are electrostatic attractions between ions with opposite charges. Ionic compounds are rigid and brittle when solid and may dissociate into their constituent ions in water. Covalent compounds, by contrast, remain intact unless a chemical reaction breaks them.
Opposing Charges Hold Ions Together in Ionic Compounds
Ionic bonds are reversible electrostatic interactions between ions...
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...