Identifying the Mechanism of Continued Growth of the Solid-Electrolyte Interphase
Fabian Single1,2, Arnulf Latz1,2,3, Birger Horstmann1,2
1German Aerospace Center (DLR), Pfaffenwaldring 38-40, 70569, Stuttgart, Germany.
Abstract:
Continued growth of the solid-electrolyte interphase (SEI) is the major reason for capacity fade in modern lithium-ion batteries. This growth is made possible by a yet unidentified transport mechanism that limits the passivating ability of the SEI towards electrolyte reduction. We, for the first time, differentiate the proposed mechanisms by analyzing their dependence on the electrode potential. Our calculations are compared to recent experimental capacity-fade data. We show that the potential dependence of SEI growth facilitated by solvent diffusion, electron conduction, or electron tunneling qualitatively disagrees with the experimental observations. Only diffusion of Li interstitials results in a potential dependence matching the experiments. Therefore, we identify the diffusion of neutral radicals, such as Li interstitials, as the cause of long-term SEI growth.
More Related Videos
10:36Electric-field Control of Electronic States in WS2 Nanodevices by Electrolyte Gating
Published on: April 12, 2018
16:27Biophysical Assays to Probe the Mechanical Properties of the Interphase Cell Nucleus: Substrate Strain Application and Microneedle Manipulation
Published on: September 14, 2011
Related Concept Videos
Interphase
Interphase
Phases of Interphase
Following each period of mitosis and cytokinesis, eukaryotic cells enter interphase, during which they grow and replicate...
Electrolyte and Nonelectrolyte Solutions
Electrolytes: van't Hoff Factor
The colligative properties of a solution depend only on the number, not on the identity, of solute species dissolved. The concentration terms in the equations for various colligative properties (freezing point depression, boiling point elevation, osmotic pressure) pertain to all solute species present in the solution. Nonelectrolytes dissolve physically without dissociation or any other accompanying process. Each molecule that dissolves yields one...
Network Covalent Solids
To break or to melt a covalent network solid, covalent bonds must be broken. Because covalent bonds are relatively strong, covalent network solids are typically...
Metallic Solids
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability....