Identification and quantitation of semi-crystalline microplastics using image analysis and differential scanning

Mauricio Rodríguez Chialanza1,2, Ignacio Sierra3, Andrés Pérez Parada3

  • 1Centro Universitario Regional del Este (CURE), Universidad de la República (UdelaR), Ruta 9 y Ruta 15, 27000, Rocha, Uruguay. mrodriguez@cure.edu.uy.

Related Concept Videos

Constant Pressure Calorimetry03:02

Constant Pressure Calorimetry

Calorimetry is a technique used to measure the amount of heat involved in a chemical or physical process or to measure the heat transferred to or from a substance. The heat is exchanged with a calibrated and insulated device called the calorimeter. Calorimetry experiments are based on the assumption that there is no heat exchange between the insulated calorimeter and the external environment. The well-insulated calorimeters prevent the transfer of heat between the calorimeter and its external...
97.9K
Calorimetry01:19

Calorimetry

When objects at different temperatures are placed in contact with each other but isolated from everything else, they attain thermal equilibrium. A container that prevents heat transfer in or out is called a calorimeter, and the use of a calorimeter to make measurements is called calorimetry. Generally, these measurements involve heat or specific heat capacity. The term "calorimetry problem" is used for any problem where the specified objects are thermally isolated from their...
4.5K
Quantitative Analysis01:12

Quantitative Analysis

Quantitative analysis is a technique for measuring the amount of specific constituents in a sample. When the sample's composition is unknown, qualitative analysis is performed first to identify its components, which ensures that the correct substances are measured during the quantitative phase.
In quantitative analysis, two key measurements are made: the sample quantity and a property proportional to the amount of the analyte (the substance being analyzed). This forms the basis of the...
1.5K
Polymer Classification: Crystallinity01:21

Polymer Classification: Crystallinity

Unlike ionic or small covalent molecules, polymers do not form crystalline solids due to the diffusion limitations of their long-chain structures. However, polymers contain microscopic crystalline domains separated by amorphous domains.
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
4.0K
Constant Volume Calorimetry02:41

Constant Volume Calorimetry

Calorimeters are useful to determine the heat released or absorbed by a chemical reaction. Coffee cup calorimeters are designed to operate at constant (atmospheric) pressure and are convenient to measure heat flow (or enthalpy change) accompanying processes that occur in solution at constant pressure. A different type of calorimeter that operates at constant volume, colloquially known as a bomb calorimeter, is used to measure the energy produced by reactions that yield large amounts of heat and...
30.9K
Leaky Scanning02:28

Leaky Scanning

During most eukaryotic translation processes, the small 40S ribosome subunit scans an mRNA from its 5' end until it encounters the first start AUG codon. The large 60S ribosomal subunit then joins the smaller one to initiate protein synthesis. The location of the translation initiation is largely determined by the nucleotides near the start codon as there may be multiple translation initiation sites present on the mRNA.  Marilyn Kozak discovered that the sequence RCCAUGG (where R...
5.7K