Color stability of nonpigmented and pigmented maxillofacial silicone elastomer exposed to 3 different environments
Ariane Farah1, Martyn Sherriff2, Trevor Coward3
1Doctoral student, Academic Centre for Reconstructive Science, King's College London, Guy's Hospital, London, United Kingdom.
Statement Of Problem:
The color degradation of maxillofacial prostheses in clinical service requires their frequent renewal. How different materials compare is unclear.
Purpose:
The purpose of this in vitro study was to investigate the color stability of a nonpigmented and pigmented maxillofacial silicone when stored in darkness and exposed to accelerated aging in a weathering chamber and natural outdoor weathering.
Material And Methods:
M511 elastomer was colored with Spectromatch Pro colorants, stored in darkness, and exposed to accelerated aging and natural outdoor weathering for 1500 hours. Test groups included nonpigmented specimens (n=18), individually pigmented specimens (n=90), and Caucasian skin tone-colored specimens (n=18). The CIELab values of the test specimens were measured using the CM-2600d spectrophotometer (Konica Minolta Sensing) at base line (0 hours) and then every 100 hours up to 1500 hours of aging. Color changes (ΔE) were calculated based on the recorded CIELab values. All data were analyzed by using linear mixed models and the Šídák multiple comparison of means test (α=.05).
Results:
A significant effect of time was found on the ΔE of all test specimens in all environments (P=.001). All pigmented M511 specimens demonstrated good color stability with maximum ΔE below the acceptability threshold of 2 ΔE when stored in darkness and exposed to outdoor weathering. However, nonpigmented specimens crossed this acceptability threshold when exposed to outdoor weathering with maximum ΔE values of 3.65. The greatest color changes were observed for all specimens when exposed to accelerated aging and most exceeded the acceptability threshold. Nonpigmented (ΔE, 4.86) and Indian yellow (ΔE, 5.20) demonstrated the highest color changes after 1500 hours.
Conclusions:
All environments resulted in visible color changes of nonpigmented and pigmented M511 elastomer. The lowest ΔE values were observed for specimens stored in darkness and the greatest for specimens exposed to accelerated aging. The organic pigment Logwood maroon demonstrated the best color stability with maximum ΔE values below the perceptibility threshold (PT) of 1 ΔE.
More Related Videos
Related Concept Videos
Colors and Magnetism
When atoms or molecules absorb light at the proper frequency, their electrons are excited to higher-energy orbitals. For many main group atoms and molecules, the absorbed photons are in the ultraviolet range of the electromagnetic spectrum, which cannot be detected by the human eye. For coordination compounds, the energy difference between the d orbitals often allows photons in the visible range to be absorbed and emitted, which is seen as colors by the human...
Color Vision
mRNA Stability and Gene Expression
Cis-acting Elements involved in mRNA stability
Nuclear Stability
To hold positively charged protons together...
Pigmentation
Melanin occurs in two primary forms: eumelanin that provides black and brown pigment and pheomelanin that provides red color. Dark-skinned individuals produce more melanin than those with pale...
RNA Stability