Biohybrid cellulose fibers: Toward paper materials with wet strength properties
Gino Mangiante1, Pierre Alcouffe2, Marianne Gaborieau3
1Université de Lyon, F-69631, Lyon; INSA Lyon, F-69621, UMR CNRS 5223, Ingénierie des Matériaux Polymères F-69621, Villeurbanne, France; Centre Technique du Papier, Domaine Universitaire, CS 90251, 38044, Grenoble Cedex 9, France.
Abstract:
Herein, we report on the preparation of novel cellulose-PEG biohybrid papers with wet strength properties. The biohybrid paper sheets are obtained using a two-step procedure where ω- or α, ω-azide functionalized PEG chains are anchored onto alkyne-functionalized wood fibers through CuAAC ligation in mild and aqueous conditions. The incorporation of the PEG grafts mostly occurs at the periphery of the cellulose fibers and degrees of substitution up to 0.028 are obtained. The presence of PEG grafts significantly increases the tensile, burst and tear strength properties in the wet state, the reinforcement being more pronounced for fibers grafted with α,ω-azide PEG. This reinforcement is consistent with a relatively sparse hetero-crosslink reaction creating inter-fiber covalent bonds and forming a cellulose network within the cell wall.
More Related Videos
Related Concept Videos
Acid Strength and Molecular Structure
In the absence of any leveling effect, the acid strength of binary compounds of hydrogen with nonmetals (A) increases as the H-A bond strength decreases down a group in the periodic table. For group 17, the order of increasing acidity is HF < HCl < HBr < HI. Likewise, for group 16, the order of increasing acid strength is H2O < H2S < H2Se < H2Te. Across a row in the periodic table, the acid strength of binary hydrogen compounds increases with increasing...
Cellulose and Pectic Polysaccharides
As a cell matures, its cell wall specializes according to its type. For example, the...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Relation Between Tensile Strength and Compressive Strength of Concrete
The Equilibrium Binding Constant and Binding Strength
Classification of Skeletal Muscle Fibers
Slow-Twitch Muscle Fibers
Slow oxidative, muscle fibers appear red due to large numbers of capillaries and high levels of...