Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: Conventional ceramic etching vs etch
Maitê Munhoz Scherer1, Catina Prochnow1, Andressa Borin Venturini1
1MSciD and PhD Post-Graduate Program in Oral Science (Prosthodontics Units), Faculty of Dentistry, Federal University of Santa Maria (UFSM), Marechal Floriano Peixoto Street, 1184, Centro, 97015372, Santa Maria, Rio Grande do Sul State, Brazil.
Objectives:
To evaluate the effect of different glass-ceramic surface treatments and aging on the fatigue failure load of a lithium disilicate glass-ceramic adhesively cemented to a dentin analogue material.
Methods:
One hundred and twenty (120) disc-shaped lithium disilicate specimens (Ø=10mm, thickness=1.5mm) were produced and randomly allocated (n=20) into 6 groups, considering 2 study factors: "surface treatment" in 3 levels (SIL-silane application only; HF5+SIL-5% hydrofluoric acid etching and silane application; ME&P-etching with an one-step ceramic primer), and "storage" in 2 levels (baseline-storage for 7 days; aging-storage for 90 days+12,000 thermal cycles). Ceramic discs were adhesively cemented to discs of a dentin analogue material (Ø=10mm, thickness=2.0mm) following the manufacturers' instructions. The fatigue failure load was determined by the staircase approach (250,000 cycles; 20Hz; initial load=1050N [∼70% of mean load-to-failure]; step size=52.5N [5% of initial load]). Micro-morphologic, fractographic, and atomic force microscope analysis were also performed. Fatigue failure load data were evaluated by one-way ANOVA, Bonferroni and t-tests for independent samples.
Results:
HF5+SIL presented higher fatigue failure load in both conditions (baseline and aging); ME&P presented intermediary mean values, while the SIL group presented the worst performance. All groups had a statistically significant decrease in the fatigue performance after aging.
Significance:
Hydrofluoric acid followed by silane application showed the best fatigue performance for an adhesively-cemented lithium disilicate ceramic. Aging negatively influenced the fatigue performance for all tested groups.
Related Concept Videos
Hydration of Cement
Soundness of Cement
Fatigue
The Looking Glass Self
Adhesion
Capillary action is a result of water’s adhesive tendencies. When a narrow...
Sign Convention
The normal force acts perpendicular to the beam's cross-section and can...