Fractographic Analysis of Brinar 400 and Brinar 500 Steels in Impact Testing

Beata Białobrzeska1, Łukasz Konat1, Robert Jasiński1

  • 1Department of Materials Science, Welding and Strength of Materials, Wrocław University of Technology, Wrocław, Poland.

Scanning
|June 2, 2018
PubMed

Related Concept Videos

Steel Fastening Techniques01:17

Steel Fastening Techniques

Steel sections can be joined together through various fastening techniques including riveting, bolting, and welding, each suitable for different structural requirements and conditions.
Rivets are cylindrical steel fasteners with a specially designed head. During application, rivets are heated until white-hot and then inserted through pre-drilled holes in the steel sections. A pneumatic hammer is used to shape the exposed end into a second head, securing the sections together.
Bolting is another...
1.3K
Steel Manufacturing01:26

Steel Manufacturing

Steel manufacturing is a multi-stage process that begins by smelting iron ore into cast iron in a blast furnace. This initial stage involves layering iron ore with coke, a type of fuel, and crushed limestone within the furnace. The coke is ignited with a high volume of air, leading to the creation of carbon monoxide, which acts to reduce the iron ore to pure iron.
During this smelting process, limestone plays a crucial role by forming slag. Slag captures impurities within the molten iron, such...
1.5K
Structural Steel Products01:24

Structural Steel Products

Structural steel products are created within a structural mill. The process begins with a beam blank that is reheated and then fed through a series of rollers. These rollers progressively shape the metal into its final form. Adjusting the spacings between the rollers allows for the production of different sections with the same nominal dimensions.
Once shaped, the steel's final form emerges as a continuous length, which is then segmented by a hot saw into manageable pieces. These segments...
693
Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
1.1K
Impact of Groups on Groups01:19

Impact of Groups on Groups

Social psychologists analyze how groups influence one another, shaping social structures and interactions through both cooperation and competition. These dynamics manifest in various ways, ranging from economic partnerships to intergroup conflicts that shape societal structures and perceptions.Cooperation and Competition in Intergroup RelationsIntergroup relationships vary across contexts, sometimes fostering cooperation and mutual benefit while at other times leading to conflict and...
258
Impact01:30

Impact

Impact occurs when two bodies collide, leading to the application of impulsive forces between them. Analyzing impact mechanics involves considering two colliding particles moving along a line known as the line of impact, which passes through their centers and is perpendicular to the contact plane.
When particles with different initial velocities collide, they induce deformation by applying equal and opposite impulses. At the point of maximum deformation, the particles move together with...
509