Aluminum dihydride complexes and their unexpected application in atomic layer deposition of titanium carbonitride

Kyle J Blakeney1, Philip D Martin, Charles H Winter

  • 1Department of Chemistry, Wayne State University, 5101 Cass Avenue, Detroit, Michigan, USA. chw@chem.wayne.edu.

Related Concept Videos

Atomic Structure01:33

Atomic Structure

Overview
210.3K
Atomic Mass01:52

Atomic Mass

Atoms — and the protons, neutrons, and electrons that compose them — are extremely small. For example, a carbon atom weighs less than 2 × 10−23 g. When describing the properties of tiny objects such as atoms, we use appropriately small units of measure, such as the atomic mass unit (amu). The amu was originally defined based on hydrogen, the lightest element, then later in terms of oxygen. Since 1961, it has been defined with regard to the most abundant isotope of carbon, atoms of which...
70.4K
Atomic Orbitals02:44

Atomic Orbitals

An atomic orbital represents the three-dimensional regions in an atom where an electron has the highest probability to reside. The radial distribution function indicates the total probability of finding an electron within the thin shell at a distance r from the nucleus. The atomic orbitals have distinct shapes which are determined by l, the angular momentum quantum number. The orbitals are often drawn with a boundary surface, enclosing densest regions of the cloud.
44.6K
Hybridization of Atomic Orbitals I03:24

Hybridization of Atomic Orbitals I

The mathematical expression known as the wave function, ψ, contains information about each orbital and the wavelike properties of electrons in an isolated atom. When atoms are bound together in a molecule, the wave functions combine to produce new mathematical descriptions that have different shapes. This process of combining the wave functions for atomic orbitals is called hybridization and is mathematically accomplished by the linear combination of atomic orbitals. The new orbitals that...
67.7K
The Quantum-Mechanical Model of an Atom02:45

The Quantum-Mechanical Model of an Atom

Shortly after de Broglie published his ideas that the electron in a hydrogen atom could be better thought of as being a circular standing wave instead of a particle moving in quantized circular orbits, Erwin Schrödinger extended de Broglie’s work by deriving what is now known as the Schrödinger equation. When Schrödinger applied his equation to hydrogen-like atoms, he was able to reproduce Bohr’s expression for the energy and, thus, the Rydberg formula governing hydrogen spectra.
59.0K
The Energies of Atomic Orbitals03:21

The Energies of Atomic Orbitals

In an atom, the negatively charged electrons are attracted to the positively charged nucleus. In a multielectron atom, electron-electron repulsions are also observed. The attractive and repulsive forces are dependent on the distance between the particles, as well as the sign and magnitude of the charges on the individual particles. When the charges on the particles are opposite, they attract each other. If both particles have the same charge, they repel each other.
30.3K