Effect of thermal cycling on fracture toughness of CAD/CAM materials
Thiago Soares Porto1, Renato Cassio Roperto1, Anna Akkus1
1Department of Comprehensive Care, School of Dental Medicine, Case Western Reserve University, Cleveland, Ohio, USA.
Purpose:
To compare the fracture toughness of four different CAD/CAM materials, (VM) Vitablocs Mark II, (IP) IPS e.max CAD, (LU) LAVA Ultimate, and (VE) Vita Enamic under long thermocycling conditions.
Methods:
Each type of ceramic block was sectioned into beams (n=9) with dimensions of 14×3×2.5 mm (L × W × H). All four ceramics were submitted to different conditions: the desiccator or distilled water, each for 7 days. The third and fourth conditions involved the specimens being submitted to 60,000 and 120,000 thermocycles in water respectively. The dwelling time was 52 seconds at 5° and 55°C. A three-point bend test with a universal loading machine on notched samples was per-formed. Furthermore, a fractographic analyses was made by scanning electron microscopy (SEM) to determine if any of these conditions influenced the type of fracture. Data were analyzed by two-way ANOVA (α= 0.05).
Results:
A significant difference in fracture toughness (P< 0.05) was found among the groups; IP (4.20±1.23) had the highest value followed by VE (2.02±0.39), which did not have a statistically significant difference from LU (1.96±0.42). The lower value and statistical difference for VM was 1.52±0.35. The ceramics performed better after they were hydrated, while the polymer-based materials had the fracture toughness means decreased after the thermocycles.
Clinical Significance:
A significant difference in fracture toughness (P<0.05) was found among the groups; IP had the highest value followed by VE, which was not statistically significantly different from LU. The ceramics performed better after they were hydrated, while the polymer-based materials had fracture toughness means decreased after thermocycling.
More Related Videos
Related Concept Videos
C4 Pathway and CAM
C4 Pathway
The C4 pathway is used by plants such as...
Toughness and Hardness of Aggregate
Lytic Cycle of Bacteriophages
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55...
What are Biogeochemical Cycles?
The Water Cycle